WE OFFER AFTER-MARKET SLURRY PUMP PARTS IN CORROSION/EROSION WEAR RESISTANT ALLOYS. SOME OF THE ALLOYS POURED ARE:
NIHARD 4. . . Meets ASTM A532, Class I, Type D Chemical Analysis
requirements.
Has highest strength and greatest resistance to impact of
all the "Nihard" family.
POLOX 700. . .
An alloy of the Nihard 4 family providing a hardness
level of 700-744 Brinell.
Close control of chemistry and special heat treatment
results in improved
abrasion resistance.
ULTRA-CHROMIUM IRON (36% HCR) .
. .High-Chromium Iron similar to ASTM A532, Class III, Type "A". A low Carbon alloy containing additional molybdenum for 700-750BH. Better corrosion
resistance
than Nihard alloys.
CORROSION/EROSION AND HEAT RESISTANT ALLOYS COMMONLY POURED AT OUR FOUNDRIES ARE USED IN MINING OPERATIONS, FERTILIZER PLANTS, COAL FIRED POWER PLANTS, CHEMICAL AND PETROCHEMICAL PLANTS.